Introduction

HXFR-PC/ABS803-T consists of environment friendly flame retardant system of bromine, passed the evaluation of SGS, CTI etc. certification authority and comply with EU ROHS requirement. Advantages: good compatibility with PC/ABS, high effective, anti-yellowing, oxidative resistance, no mold corrosion, non-blooming, high smoothness and good low-temperature toughness.

Application

Mainly used in imported fire-retardant PC/ABS recycled material injection and modification. parts of computer, Electric meter, connecter, enclosure of notebook or mouse.

Index

Item

Index

Appearance

White Granular

Density g/cm3

1.42

Decomposition Temp ℃≥

300

Content %>

52

Water Content %≤

0.1

Recommended Dosage

100:10

Solubility Index g/min,200℃5kg

40

Melting Temp ℃≥

140

Extrusion Process (Twin Screw Extruder)

Note: Vacuum when production; Recommended Screw L/D 1:36-40;

Packing/Storage

25KG/bag: Transported as a common chemical and stored in dry and cool place, avoid direct sunlight.

Appendix:Application Examples

1-1.Formula

Materials

Formula A

Fire-retardant PC/ABS Recycling Materials

100

HXFR-PC/ABS803-T

10

1-2.Technical Data

Properties

Test Methods

Unit

 Recycling Materials

Formula A

Density

ASTMD-792

g/cm3

1.2

1.22

Melt Index(200℃5KG)

ASTMD-955

g/10min

-

-

Tensile Strength

ASTM-D638

MPa

57.8

52.2

Elongation At Break

ASTM-D638

%

22.2

21.8

Flexural Strength

ASTM-D790

MPa

83.6

78

Flexural Modulus

ASTM-D790

MPa

2451.5

2297

Izod Impact Strength Notched(23℃)

ASTM-D256

KJ/m2

20.0

21.6

Flame Retardancy 1.6mm

UL94

‐‐

V1

V0

GWFI

IEC60695-2-12

Not Pass

750pass

1-3. PC/ABS Injection Process:

Drying condition: Drying at 80-100 deg C to 2-3 hours by desiccant dryers.

Injection machine temperature setup:

Heating Zone

Step1

Step2

Step3

Nozzle

Temperature

225

230

240

235

All the application typical data above are just for reference, not an official warranty certificate.Provide different design solutions according to requirement of customers.